AASHTO TP 127-17 test method covers the determination of fracture energy density of asphalt binder by means ofa direct tension test. For evaluation of relative cracking performance, it is recommended that thistest procedure be used with asphalt binder aged using T 240 (RTFO) plus R 28 (PAV). However,this test can be used for determination of binder facture energy for any binder including any aged(RTFO plus PAV or PAV only) neat or modified binder and asphalt binder extracted andrecovered from pavement. The test apparatus is designed for testing within the intermediatetemperature range, from 0°C to 25°C.